Nickel Alloys

  • RA330®

    Inventory: PlateExpanded MetalHex NutsRod CoilPipeTubingWeld WireThreaded BarRound BarWashersSheet

    RA330® - The workhorse of austenitic heat resistant alloys. Good strength, carburization and oxidation resistance up to 2100°F.
     CrNiSiCMnPSCuFe
    MIN 18.00 34.00 1.00 -- -- -- -- -- Balance
    MAX 20.00 37.00 1.50 0.08 2.00 0.03 0.03 1.00  
  • RA333®

    Inventory: PlateWeld Wire

    RA333® - A nickel base superalloy with excellent carburization, oxidation, and hot corrosion resistance. It has high creep rupture strength with exceptional ability to withstand repeated thermal shock.
     NiCrMoCoWSiMnCFe
    MIN 44.00 24.00 2.50 2.50 2.50 0.75 -- --  
    MAX 47.00 27.00 4.00 4.00 4.00 1.50 2.00 0.08 Balance
  • RA 602 CA®

    Inventory: PlateWeld WireSheet

    RA 602 CA® - One of the most oxidation resistant high strength, heat resistant nickel alloys available. Useful through 2200°F.
     CrNiCAlTiYZrMnSiCuFe
    MIN 24.00   0.15 1.80 0.10 0.05 0.01 -- -- -- 8.00
    MAX 26.00 Balance 0.25 2.40 0.20 0.12 0.10 0.15 0.50 0.10 11.00
  • 600

    Inventory: PlateRod CoilPipeWeld WireRound BarSheet

    Inconel 600 - A nickel-chromium alloy with good carburization and oxidation resistance through 2000°F.
     NiCrCMnCuSiSFe
    MIN 72.00 14.00 -- -- -- -- -- 6.00
    MAX   17.00 0.15 1.00 0.50 0.50 0.015 10.00

    *ASTM specification 0.20 max C.

  • 601

    Inventory: PlatePipeSheet

    601 is a nickel-base alloy with high chromium and an aluminum addition. Outstanding oxidation resistance to 2200°F, good strength and carburization resistance.
     NiCrAlCMnCuSiSFe
    MIN 58.00 21.00 1.00 -- -- -- -- -- --
    MAX 63.00 25.00 1.70 0.10 1.00 1.00 0.50 0.015 Balance

    *ASTM specification 0.20 max C.

  • 625

    Inventory: PlateRound BarSheet

    625 alloy is high creep-rupture strength, oxidation resistant to 1800°F (982°C). Excellent resistance to hot seawater, scrubber environments and reducing acids.
     CrNiMoCoCb+TaAlTiCFeMnSiPS
    MIN 20.0 - 8.0 - 3.15 - - - - - - - -
    MAX 23.0 Balance 10.0 1.0 4.15 0.4 0.4 0.1 5.0 0.5 0.5 0.015 0.015
  • 718

    Inventory: PlateRound BarSheet

    Inconel 718 - Nickel alloy precipitation hardened by gamma prime and double prime. Readily fabricated, weldable even in the hardened condition. Used for gas turbine components to 1200°F, as well as for cryogenic equipment.
     Ni+CoCrCb+TaMoTiAlCoCMnSiPSBCuFe
    MIN 50.00 17.00 4.75 2.80 0.65 0.20 -- -- -- -- -- -- -- -- --
    MAX 55.00 21.00 5.50 3.30 1.15 0.80 1.00 0.08 0.35 0.35 0.015 0.015 0.006 0.30 Balance
  • 718 (AMS 5663)

    Inventory: Round Bar

    Alloy 718 (AMS 5663) is bar that is already aged (precipitation hardened). As supplied, this material provides high tensile strength and hardness compared to 718 in the annealed condition.
  • Alloy X

    Inventory: PlateRound BarSheet

    Alloy X - Good strength and ease of fabrication, with excellent oxidation resistance through 2000°F. Widely used for aircraft, marine and industrial gas turbine combustors.
     CrMoCoWAlTiBCFeMnSiPSCuNi
    MIN 20.5 8.0 0.5 0.2 - - - 0.05 17.0 - - - - - -
    MAX 23.0 10.0 2.5 1.0 0.5 0.15 0.01 0.15 20.0 1.0 1.0 0.04 0.03 0.5 Balance
  • INVAR 36

    Inventory: Plate

    INVAR 36 is a nickel-iron, low-expansion alloy containing 36% nickel. Used for molds and dies to form composites.
     NiFeMoCCuMnSiPSCr
    MIN 35.0 - - - - - - - - -
    MAX 37.0 Balance 0.5 0.1 0.5 0.6 0.35 0.025 0.025 0.5
  • AL-6XN®

    Inventory: PlateTeesConcentric ReducersForged BilletPipeStub EndsFittingsRound BarSheet

    AL-6XN® alloy (UNS N08367) is a low carbon, high purity, nitrogen-bearing "super-austenitic" stainless alloy. The AL6XN alloy was designed to be a seawater resistant material and has since been demonstrated to be resistant to a broad range of very corrosive environments.
     CrNiMoCNMnSiPSCuFe
    MIN 20.00 23.50 6.00 -- 0.18 -- -- -- -- --  
    MAX 22.00 25.50 7.00 0.03 0.25 2.00 1.00 0.04 0.03 0.75 Balance
  • 800H/AT

    Inventory: PlateSheet

    800 H/AT - High strength austenitic heat resistant alloy for ASME code applications to 1650°F.
     CrNiMnSiAlTiAl +TiCCuPSFe
    MIN 19.0 30.0 - - 0.15 0.15 0.85 0.06 - - - 39.5
    MAX 23.0 35.0 1.5 1.0 0.6 0.6 1.2 0.1 0.75 0.045 0.015 -
  • Alloy 20

    Inventory: PlateWeld WireSheet

    Alloy 20 - The alloy designated specifically to withstand sulfuric acid. Practical immunity to chloride stress corrosion cracking. Stabilized to prevent intergranular corrosion as welded. Resistant to polythionic acid SCC.
     NiCrMoMnCuSiCSPCb+TaFe
    MIN 32.5 19.0 2.0 - 3.0 - - - - 8.0 x C 1.0 -
    MAX 35.0 21.0 3.0 2.0 4.0 1.0 0.06 0.035 0.035 - Balance
  • 230®

    Inventory: Sheet

    230 - High strength nickel based alloy used for land based gas turbines.
     NiCrWMoCoAlLaMnCSiPhSBTiCuFe
    MIN 47.00 20.00 13.00 1.00 - 0.20 0.005 0.30 0.05 0.25 - - - - - -
    MAX 65.00 24.00 15.00 3.00 5.00 0.50 0.005 1.00 0.15 0.75 0.03 0.015 0.015 0.10 0.50 3.00