INVAR 36

INVAR 36 is a nickel-iron, low-expansion alloy containing 36% nickel. It maintains nearly constant dimensions over the range of normal atmospheric temperatures, and has a low coefficient of expansion from cryogenic temperatures to about 500°F. The alloy also retains good strength and toughness at cryogenic temperatures. INVAR 36 can be hot and cold formed and machined using processes similar to austenitic stainless steels. 

Inventory

INVAR 36 Plate

Common Trade Names

Nilo 36

Features

  • Low expansion rate up to 500°F
  • Readily weldable

Applications

  • Tooling and dies for composite forming
  • Cryogenic components
  • Laser components