What is a Timesavers machine?

A Timesavers machine is used for fast production deburring of finished laser-cut metal parts.

How does it work?

A Timesavers machine runs similarly to a belt sander to deburr the edge of parts. It provides a clean, consistent finish across the entire work surface. The dry Timesavers is used for Stainless and nickel alloys while the wet Timesavers is used on titanium alloys.

Capabilities

  • Used for grinding/sanding/deburring
  • Both wet and dry options available
  • .015" min thickness
  • 36" max width
  • 1" x 3" minimum